固溶时效对激光沉积修复ZM6合金组织及力学性能的影响 |
| 钦兰云, 张健, 伊俊振, 崔岩峰, 杨光, 王超 |
|
Effects of Solution Aging on Microstructural Evolution and Mechanical Properties of Laser Deposition Repairing ZM6 Alloy |
| QIN Lanyun, ZHANG Jian, YI Junzhen, CUI Yanfeng, YANG Guang, WANG Chao |
| 图13 LDR与LDR-T6试样修复区晶界分布图及取向差统计图 |
| Fig.13 Grain boundary distribution maps of RZ in LDR (a) and LDR-T6 (b) samples and the corresponding misorientation statistical diagram (c) |
|