固溶时效对激光沉积修复ZM6合金组织及力学性能的影响 |
| 钦兰云, 张健, 伊俊振, 崔岩峰, 杨光, 王超 |
|
Effects of Solution Aging on Microstructural Evolution and Mechanical Properties of Laser Deposition Repairing ZM6 Alloy |
| QIN Lanyun, ZHANG Jian, YI Junzhen, CUI Yanfeng, YANG Guang, WANG Chao |
| 图9 基材、LDR与LDR-T6试样的工程应力-应变曲线、断裂位置及室温拉伸性能 |
| Fig.9 Engineering stress-strain curves (a) and tensile properties (b) of BM, LDR, and LDR-T6 samples at room temperature (Insets in Fig.8a show the fracture positions; FZ—fusion zone; UTS—ultimate tensile strength, YS—yield strength, EL—elongation) |
|