利用热轧制-剪切-弯曲工艺及退火调控Mg-Al-Zn-Mn-Ca 镁合金的织构 |
| 游云翔, 谭力, 高静静, 周涛, 周志明 |
|
Controlling the Texture of Mg-Al-Zn-Mn-Ca Magnesium Alloy by Hot Rolling-Shearing-Bending Process and Annealing |
| YOU Yunxiang, TAN Li, GAO Jingjing, ZHOU Tao, ZHOU Zhiming |
| 图8 400 ℃退火1 h后Mg-2Al-2Zn-0.4Mn-0.5Ca镁合金板材的电子背散射衍射(EBSD)像以及孪晶与相应基体的几何位置关系 |
| Fig.8 EBSD image of the selected region in Fig.4a of Mg-2Al-2Zn-0.4Mn-0.5Ca magnesium alloy sheet annealed at 400 oC for 1 h (The grey cubes represent schematic illustration of the matrix and twin) (a) and the geometric relationship between twins and their corresponding matrix positions (The black and green dashed lines represent the majority of the matrix orientation distribution, and the red dashed line represents the orientation distribution of { |
|