利用热轧制-剪切-弯曲工艺及退火调控Mg-Al-Zn-Mn-Ca 镁合金的织构 |
| 游云翔, 谭力, 高静静, 周涛, 周志明 |
|
Controlling the Texture of Mg-Al-Zn-Mn-Ca Magnesium Alloy by Hot Rolling-Shearing-Bending Process and Annealing |
| YOU Yunxiang, TAN Li, GAO Jingjing, ZHOU Tao, ZHOU Zhiming |
| 图7 拉伸前非基面织构Mg-2Al-2Zn-0.4Mn-0.5Ca 镁合金板材沿不同方向滑移系统的Schmid因子(SF)分布 |
| Fig.7 Distribution of schmid factor (SF) in basal <a> slip (a) and prismatic <a> slip (b) systems of non-basal textured Mg-2Al-2Zn-0.4Mn-0.5Ca magnesium alloy sheet in different loading directions before uniaxial tension |
|