利用热轧制-剪切-弯曲工艺及退火调控Mg-Al-Zn-Mn-Ca 镁合金的织构 |
| 游云翔, 谭力, 高静静, 周涛, 周志明 |
|
Controlling the Texture of Mg-Al-Zn-Mn-Ca Magnesium Alloy by Hot Rolling-Shearing-Bending Process and Annealing |
| YOU Yunxiang, TAN Li, GAO Jingjing, ZHOU Tao, ZHOU Zhiming |
| 图1 热轧制前铸态Mg-2Al-2Zn-0.4Mn-0.5Ca 镁合金薄片的宏观形貌 |
| Fig.1 Macroscopic photograph of the as-cast Mg-2Al-2Zn-0.4Mn-0.5Ca magnesium alloy sheets before hot rolling |
|