Ti30Ni50Hf20 高温形状记忆合金的热变形行为 |
| 姜沐池, 宫继双, 杨兴远, 任德春, 蔡雨升, 李秉洋, 吉海宾, 雷家峰 |
|
Hot Deformation Behavior of Ti30Ni50Hf20 High-Temperature Shape Memory Alloy |
| JIANG Muchi, GONG Jishuang, YANG Xingyuan, REN Dechun, CAI Yusheng, LI Bingyang, JI Haibin, LEI Jiafeng |
| 图9 应变速率为0.01 s-1时不同变形温度下Ti30Ni50Hf20高温形状记忆合金显微组织的OM像 |
| Fig.9 OM images for Ti30Ni50Hf20 high-temperature shape memory alloy at strain rate of 0.01 s-1 at deformation temperatures of 700 oC (a), 800 oC (b), and 900 oC (c) |
|