Ti30Ni50Hf20 高温形状记忆合金的热变形行为 |
| 姜沐池, 宫继双, 杨兴远, 任德春, 蔡雨升, 李秉洋, 吉海宾, 雷家峰 |
|
Hot Deformation Behavior of Ti30Ni50Hf20 High-Temperature Shape Memory Alloy |
| JIANG Muchi, GONG Jishuang, YANG Xingyuan, REN Dechun, CAI Yusheng, LI Bingyang, JI Haibin, LEI Jiafeng |
| 图6 Ti30Ni50Hf20高温形状记忆合金ln[sinh(ασp)]与1000 / T的关系 |
| Fig.6 Relationship between ln[sinh(ασp)] and 1000 / T of Ti30Ni50Hf20 high-temperature shape memory alloy |
|