Ti30Ni50Hf20 高温形状记忆合金的热变形行为 |
| 姜沐池, 宫继双, 杨兴远, 任德春, 蔡雨升, 李秉洋, 吉海宾, 雷家峰 |
|
Hot Deformation Behavior of Ti30Ni50Hf20 High-Temperature Shape Memory Alloy |
| JIANG Muchi, GONG Jishuang, YANG Xingyuan, REN Dechun, CAI Yusheng, LI Bingyang, JI Haibin, LEI Jiafeng |
| 图1 铸态Ti30Ni50Hf20高温形状记忆合金的显微组织OM像和DSC曲线及Ti50Ni50形状记忆合金的DSC曲线 |
| Fig.1 OM image (a) and DSC curve (b) for as-cast Ti30Ni50Hf20 high-temperature shape memory alloy, and DSC curve for as-cast Ti50Ni50 shape memory alloy (c) |
|