V添加对Ti2AlNb合金组织演变及硬度的影响 |
| 刘子儒, 郭乾应, 张虹雨, 刘永长 |
|
Effects of V on the Microstructure Evolution and Hardness Enhancement of Ti2AlNb Alloy |
| LIU Ziru, GUO Qianying, ZHANG Hongyu, LIU Yongchang |
| 图12 Ti-22Al-25Nb-1V合金中弯曲组织的TEM分析 |
| Fig.12 TEM image (a) and corresponding SAED patterns of regions A (b) and B (c) in Fig.12a showing the curved microstructure for the Ti-22Al-25Nb-1V alloy after solution treatment at 1300 ºC and aging at 850 ºC |
|