V添加对Ti2AlNb合金组织演变及硬度的影响 |
| 刘子儒, 郭乾应, 张虹雨, 刘永长 |
|
Effects of V on the Microstructure Evolution and Hardness Enhancement of Ti2AlNb Alloy |
| LIU Ziru, GUO Qianying, ZHANG Hongyu, LIU Yongchang |
| 图10 Ti-22Al-25Nb和Ti-22Al-25Nb-1V合金在850 ℃时效后的TEM像 |
| Fig.10 TEM images of Ti-22Al-25Nb (a) and Ti-22Al-25Nb-1V (b) alloys after solution treatment at 1300 ºC and aging at 850 ºC (Inset in Fig.11b shows the SAED pattern of region A) |
|