V添加对Ti2AlNb合金组织演变及硬度的影响 |
| 刘子儒, 郭乾应, 张虹雨, 刘永长 |
|
Effects of V on the Microstructure Evolution and Hardness Enhancement of Ti2AlNb Alloy |
| LIU Ziru, GUO Qianying, ZHANG Hongyu, LIU Yongchang |
| 图9 Ti-22Al-25Nb-1V合金在900 ℃时效后的SEM背散射电子(BSE)像以及相应的EDS线扫描结果 |
| Fig.9 SEM backscattered electron (BSE) image (a) and corresponding linear scan analyses alone the line in Fig.9a (b) of the Ti-22Al-25Nb-1V alloy after solution treatment at 1300 ºC and aging at 900 ºC |
|