V添加对Ti2AlNb合金组织演变及硬度的影响 |
| 刘子儒, 郭乾应, 张虹雨, 刘永长 |
|
Effects of V on the Microstructure Evolution and Hardness Enhancement of Ti2AlNb Alloy |
| LIU Ziru, GUO Qianying, ZHANG Hongyu, LIU Yongchang |
| 图3 Ti-22Al-25Nb合金经过不同温度时效处理后的SEM像 |
| Fig.3 SEM images of the Ti-22Al-25Nb alloy after solution treatment at 1300 ºC and aging at 800 ºC (a), 850 ºC (b), 900 ºC (c), 950 ºC (d), 1000 ºC (e), and 1050 ºC (f) |
|