V添加对Ti2AlNb合金组织演变及硬度的影响 |
| 刘子儒, 郭乾应, 张虹雨, 刘永长 |
|
Effects of V on the Microstructure Evolution and Hardness Enhancement of Ti2AlNb Alloy |
| LIU Ziru, GUO Qianying, ZHANG Hongyu, LIU Yongchang |
| 图1 Ti-22Al-25Nb和Ti-22Al-25Nb-1V合金1300 ℃固溶后的XRD谱 |
| Fig.1 XRD spectra of Ti-22Al-25Nb and Ti-22Al-25Nb-1V alloys after solution treatment at 1300 ºC |
|