低合金化Mg-Ag镁空气电池阳极材料的电化学行为和放电性能 |
| 郝旭邦, 程伟丽, 李戬, 王利飞, 崔泽琴, 闫国庆, 翟凯, 余晖 |
|
Electrochemical Behavior and Discharge Performance of a Low-Alloyed Mg-Ag Alloy as Anode for Mg-Air Battery |
| HAO Xubang, CHENG Weili, LI Jian, WANG Lifei, CUI Zeqin, YAN Guoqing, ZHAI Kai, YU Hui |
| 图11 Q1合金在不同电流密度和不同放电时间去产物表面形貌下的SEM像和放电10 h后去产物3D形貌 |
| Fig.11 Surface SEM images of Q1 alloy discharged at different current densities for 10 min (a, f), 30 min (b, g), 1 h (c, h), 10 h (d, i) after removing the discharge products; and 3D morphologies of Q1 alloy discharged for 10 h after removing the discharge products (e, j) (Insets show the high magnified images) (a-e) 2.5 mA/cm2 (f-j) 20 mA/cm2 |
|