低合金化Mg-Ag镁空气电池阳极材料的电化学行为和放电性能 |
| 郝旭邦, 程伟丽, 李戬, 王利飞, 崔泽琴, 闫国庆, 翟凯, 余晖 |
|
Electrochemical Behavior and Discharge Performance of a Low-Alloyed Mg-Ag Alloy as Anode for Mg-Air Battery |
| HAO Xubang, CHENG Weili, LI Jian, WANG Lifei, CUI Zeqin, YAN Guoqing, ZHAI Kai, YU Hui |
| 图10 Q1合金不同电流密度下放电产物的XPS |
| Fig.10 XPS of the oxide films on the alloy surface after discharge at 2.5 and 20 mA/cm2 in 3.5%NaCl solution for 10 h, including high-resolution Mg1s (a), Ag3d (b), Cl2p (c), and O1s (d) spectra |
|