低合金化Mg-Ag镁空气电池阳极材料的电化学行为和放电性能 |
| 郝旭邦, 程伟丽, 李戬, 王利飞, 崔泽琴, 闫国庆, 翟凯, 余晖 |
|
Electrochemical Behavior and Discharge Performance of a Low-Alloyed Mg-Ag Alloy as Anode for Mg-Air Battery |
| HAO Xubang, CHENG Weili, LI Jian, WANG Lifei, CUI Zeqin, YAN Guoqing, ZHAI Kai, YU Hui |
| 图7 不同电流密度下Q1合金和HP Mg的放电曲线 |
| Fig.7 Discharge curves of Q1 alloy and HP Mg at different current densities (a) 2.5 mA/cm2 (b) 5 mA/cm2 (c) 10 mA/cm2 (d) 20 mA/cm2 |
|