低合金化Mg-Ag镁空气电池阳极材料的电化学行为和放电性能 |
| 郝旭邦, 程伟丽, 李戬, 王利飞, 崔泽琴, 闫国庆, 翟凯, 余晖 |
|
Electrochemical Behavior and Discharge Performance of a Low-Alloyed Mg-Ag Alloy as Anode for Mg-Air Battery |
| HAO Xubang, CHENG Weili, LI Jian, WANG Lifei, CUI Zeqin, YAN Guoqing, ZHAI Kai, YU Hui |
| 图5 Q1合金和HP Mg的开路电位、极化曲线阳极分支和阴极分支极化曲线及Nyquist图 |
| Fig.5 Open circuit potentials (EOCP) (a), anodic (b) and cathodic (c) branches of the polarization curves, and Nyquist diagram under open circuit potentials (d) of Q1 alloy and high purity magnesium (HP Mg) (E—potential; i—current density; Z' and Z"—real part and imaginary part of the impedance, respectively; SCE—saturated calomel electrode. Inset in Fig.5d is the zoom-in view of the box area) |
|