表1 零热膨胀金属材料的热膨胀数据[14~46]
|
Table 1 Thermal expansion data of zero thermal expansion metallic materials[14-46]
|
|
| Material | Type | αl / (10-6 K-1) | Temp. range / K | Ref. |
|---|
| Fe0.65Ni0.35 | Invar | 1.5 | 193-373 | [17] | | Zr0.8Nb0.2Fe2 | AFe2 | 1.4 | 3-470 | [18] | | (Zr0.65Nb0.35)0.95Fe0.05Fe2 | | 0.47 | 4-425 | [19] | | Zr0.8Ta0.2Fe1.7Co0.3 | | 0.21 | 100-360 | [20] | | Zr0.7Ta0.3Fe2 | | 0.9 | 10-430 | [21] | | Sc0.55Ti0.45Fe2 | | 0.41a | 10-250 | [22] | | Sc0.725Nb0.275Fe2 | | 0.69 | 108-264 | [23] | | HfFe2.5 | | 0.42a | 433-583 | [24] | | Hf0.8Nb0.2Fe2.5 | | 0.06a | 250-380 | [25] | | Hf0.6Ti0.4Fe2.5 | | 0.53a | 100-450 | [26] | | Hf0.85Ta0.15Fe2C0.01 | | 0.8a | 85-245 | [27] | | Tb(Co1.9Fe0.1) | RCo2 | 0.48 | 123-307 | [28] | | Gd0.25Dy0.75Co1.93Fe0.07 | | 0.16 | 10-275 | [29] | | Gd0.5(Ho0.5Dy0.5)0.5Co2 | | 1.3 | 5-220 | [30] | | LaFe11.0Si2.0 hydride | La(Fe, M)13 | 0.5 | 20-275 | [31] | | LaFe10.3Al2.7 | | 0.36 | 4.2-250 | [32] | | LaFe10.6Si2.4 | | -0.8 | 15-150 | [33] | | Ho2Fe16Co | R2Fe17 | 0.07a | 3-461 | [34] | | Ho2Fe16Cr | | 0.43a | 13-330 | [35] | | Er2(Fe0.95Co0.05)14B | R2Fe14B | 0.5a | 120-475 | [36] | | MnCoGe0.99In0.01 | MnCoGe | 0.68 | 200-310 | [37] | | ErFe10V1.4Mo0.6 | RFe12 | 1.6 | 120-440 | [38] | | MnFe4Si3 | Mn5Si3 | 0.45b | 10-310 | [39] | | Ni49.4Ti50.6 | Ti-based | 0.53b | 123-353 | [40] | | Ni50.8Ti49.2 | | 2.3b | 77-300 | [41] | | Ti22Nb | | 0.2b | 273-573 | [42] | | xLFCS/39.7%Cu (volume fraction) | Duplex alloy | -0.21 | 200-320 | [43] | | LaFe54Co3.5Si3.35 | | 1.10 | 260-310 | [14] | | Ho0.04Fe0.96 | | 0.19b | 100-335 | [15] | | LaFe10.1Cu0.5Si2.4 | | 0.28 | 185-250 | [44] | | Er2Fe19B1.35 | | 0.28 | 100-500 | [16] | | Fe2.75Co0.25PtB0.25 | | 0.95 | 360-560 | [45] | | Hf0.8Ta0.2Fe2.5 | | 0.352 | 265-350 | [46] |
|
|
|