钽合金表面渗碳层中碳化物析出及其性能的第一性原理研究 |
| 孟祥龙, 刘瑞良, Li D. Y. |
|
First Principles Study on the Precipitation and Properties of Carbides in the Surface Carburized Layer of Tantalum Alloys |
| MENG Xianglong, LIU Ruiliang, Li D. Y. |
| 图5 不同结构含W复合碳化钽的力学性质 |
| Fig.5 Mechanical properties of complex tantalum carbide containing W with different structures (a) modulus (b) Vickers hardness (c) G / Bvs Poisson's ratio |
|