仿生苍耳球冠织构的Ni-Co-Zn超疏水合金涂层及其抗覆冰性能 |
||||||||||||||||||||
| 周小卫, 郭云, 荆雪艳, 王宇鑫 | ||||||||||||||||||||
|
Biologically Inspired Xanthium-Like Spherical Texture in Superhydrophobic Ni-Co-Zn Coatings and Their Anti-Icing Performances |
||||||||||||||||||||
| ZHOU Xiaowei, Guo Yun, JING Xueyan, WANG Yuxin | ||||||||||||||||||||
| 表2 络合剂Na3Cit添加量为5 g/L时不同Zn2+浓度条件下Ni-Co-Zn涂层试样经不同时效处理后的WCA测量结果 (°) |
||||||||||||||||||||
| Table 2 Effects of aging temperature on WCA for Ni-Co-Zn coating within different Zn2+ concentrations in bath under Na3Cit addition of 5 g/L |
||||||||||||||||||||
|
||||||||||||||||||||