仿生苍耳球冠织构的Ni-Co-Zn超疏水合金涂层及其抗覆冰性能 |
| 周小卫, 郭云, 荆雪艳, 王宇鑫 |
|
Biologically Inspired Xanthium-Like Spherical Texture in Superhydrophobic Ni-Co-Zn Coatings and Their Anti-Icing Performances |
| ZHOU Xiaowei, Guo Yun, JING Xueyan, WANG Yuxin |
| 图10 Zn2+和络合剂 Na3Cit浓度分别为50和5 g/L条件下Ni-Co-Zn涂层经自然时效后的多触角乳突状和人工时效后的苍耳球冠织构SEM像 |
| Fig.10 Low (a, b) and high (a1, b1) magnified SEM images showing the surface features of Ni-Co-Zn coatings with multi-antenna structure after natural aging (a, a1) and xanthium-like spherical texture by ZnO whiskers after artificial aging at 200 oC (b, b1) under Zn2+ concentration of 50 g/L and Na3Cit addition of 5 g/L (Inset in Fig.12b show the EDS result of square area) |
|