仿生苍耳球冠织构的Ni-Co-Zn超疏水合金涂层及其抗覆冰性能 |
| 周小卫, 郭云, 荆雪艳, 王宇鑫 |
|
Biologically Inspired Xanthium-Like Spherical Texture in Superhydrophobic Ni-Co-Zn Coatings and Their Anti-Icing Performances |
| ZHOU Xiaowei, Guo Yun, JING Xueyan, WANG Yuxin |
| 图8 Ti基体、Zn2+和络合剂Na3Cit浓度分别为50和5 g/L条件下阳极氧化蜂窝多孔Ti和Ni-Co-Zn涂层经不同温度时效后的试样表面在-10 ℃下延迟结冰特性的OM像 |
| Fig.8 OM images of anti-icing (icing) performance tests at -10 oC on surfaces of Ti substrate (a); OM images of anodized porous template (b) and Ni-Co-Zn coatings aged at 25 oC (c), 100 oC (d), 200 oC (e), and 300 oC (f) under Zn2+ concentration of 50 g/L and Na3Cit addition of 5 g/L |
|