仿生苍耳球冠织构的Ni-Co-Zn超疏水合金涂层及其抗覆冰性能 |
| 周小卫, 郭云, 荆雪艳, 王宇鑫 |
|
Biologically Inspired Xanthium-Like Spherical Texture in Superhydrophobic Ni-Co-Zn Coatings and Their Anti-Icing Performances |
| ZHOU Xiaowei, Guo Yun, JING Xueyan, WANG Yuxin |
| 图7 Zn2+和络合剂 Na3Cit浓度分别为50和5 g/L条件下Ni-Co-Zn涂层试样经不同温度时效后在干燥空气中暴露14 d后表面形貌的SEM像 |
| Fig.7 SEM images showing surface features of Ni-Co-Zn coatings aging at room temperature (25 oC) (a), 100 oC (b), 200 oC (c), and 300 oC (d) and then exposing to air for 14 d under Zn2+ concentration of 50 g/L and Na3Cit addition of 5 g/L (Insets show the locally enlarged images) |
|