仿生苍耳球冠织构的Ni-Co-Zn超疏水合金涂层及其抗覆冰性能 |
| 周小卫, 郭云, 荆雪艳, 王宇鑫 |
|
Biologically Inspired Xanthium-Like Spherical Texture in Superhydrophobic Ni-Co-Zn Coatings and Their Anti-Icing Performances |
| ZHOU Xiaowei, Guo Yun, JING Xueyan, WANG Yuxin |
| 图1 不同直流电压下蜂窝多孔Ti表面的SEM像及其孔径分布 |
| Fig.1 SEM images (a, c, e) and correspongding pore size distributions (b, d, f) of the honeycomb-like porous surfaces of Ti matrix during anodizing at direct current voltages of 140 V (a, b), 160 V (c, d), and 180 V (e, f) |
|