一种镍基高温合金的高温HCl腐蚀行为 |
| 周一鸣, 韩勇军, 谢光, 郑伟, 肖炎彬, 潘阳, 张健 |
|
High-Temperature Corrosion Behavior of a Nickel-Based Superalloy in HCl-Containing Atmosphere |
| ZHOU Yiming, HAN Yongjun, XIE Guang, ZHENG Wei, XIAO Yanbin, PAN Yang, ZHANG Jian |
| 图12 镍基高温合金在960 ℃含5%HCl气氛中腐蚀不同时间后截面形貌的SEM-BSE像及EPMA元素面分布 |
| Fig.12 Cross sectional SEM-BSE images and corresponding EPMA element maps of the nickel-based superalloy afte corroded in 5%HCl-containing atmosphere for 25 h (a), 50 h (b), 75 h (c), and 100 h (d) at 960 oC |
|