一种镍基高温合金的高温HCl腐蚀行为
周一鸣, 韩勇军, 谢光, 郑伟, 肖炎彬, 潘阳, 张健

High-Temperature Corrosion Behavior of a Nickel-Based Superalloy in HCl-Containing Atmosphere
ZHOU Yiming, HAN Yongjun, XIE Guang, ZHENG Wei, XIAO Yanbin, PAN Yang, ZHANG Jian
图9 镍基高温合金在960 ℃含5%HCl气氛中腐蚀不同时间后截面形貌的SEM-BSE像
Fig.9 Cross sectional SEM-BSE images of nickel-based superalloy after corrosion in 5%HCl-containing atmosphere for 25 h (a), 50 h (b), 75 h (c), 100 h (d), and 200 h (e) at 960 oC (TCP—topologically close-packed)