一种镍基高温合金的高温HCl腐蚀行为
周一鸣, 韩勇军, 谢光, 郑伟, 肖炎彬, 潘阳, 张健

High-Temperature Corrosion Behavior of a Nickel-Based Superalloy in HCl-Containing Atmosphere
ZHOU Yiming, HAN Yongjun, XIE Guang, ZHENG Wei, XIAO Yanbin, PAN Yang, ZHANG Jian
图7 镍基高温合金在960 ℃含5%HCl气氛中腐蚀不同时间后表面腐蚀产物的XRD谱、设备冷凝端挥发性腐蚀产物的实物图及其XRD谱
Fig.7 XRD spectra of the corrosion products on the surface of nickel-based superalloy (a) and macro morphology (b) and XRD spectra (c) of volatile corrosion products on the equipment condensing end after corrosion in 5%HCl-containing atmosphere for different time at 960 oC