一种镍基高温合金的高温HCl腐蚀行为 |
| 周一鸣, 韩勇军, 谢光, 郑伟, 肖炎彬, 潘阳, 张健 |
|
High-Temperature Corrosion Behavior of a Nickel-Based Superalloy in HCl-Containing Atmosphere |
| ZHOU Yiming, HAN Yongjun, XIE Guang, ZHENG Wei, XIAO Yanbin, PAN Yang, ZHANG Jian |
| 图6 镍基高温合金表面剥落面积随腐蚀时间的变化 |
| Fig.6 Changes of spalling area on the surface of nickel-based superalloy with corrosion time |
|