先进镍基粉末高温合金FGH4108在不同应力条件下的蠕变行为 |
| 李新宇, 白佳铭, 张浩鹏, 李晓鲲, 贾建, 刘常升, 刘建涛, 张义文 |
|
Creep Behavior of Advanced Powder Metallurgy Nickel-Based Superalloys FGH4108 Under Different Stress Conditions |
| LI Xinyu, BAI Jiaming, ZHANG Haopeng, LI Xiaokun, JIA Jian, LIU Changsheng, LIU Jiantao, ZHANG Yiwen |
| 图12 粗晶和细晶组织合金的应力敏感指数 |
| Fig.12 Stress sensitivity indexes (n) of the coarse grain and fine grain samples (σ—applied stress, R—relevance of the data) |
|