Inconel 740H焊接接头不同温度蠕变后 γ′贫化区的形成及其对力学性能的影响 |
| 周任远, 朱丽慧 |
|
Formation of γ′-Denuded Zone and Its Effect on the Mechanical Properties of Inconel 740H Welded Joint After Creep at Different Temperatures |
| ZHOU Renyuan, ZHU Lihui |
| 图6 蠕变前IN 740H焊接接头显微组织的SEM像 |
| Fig.6 SEM images of microstructures of IN 740H welded joint before creep (Inset in Fig.6c shows the corresponding EDS analysis; rectangle in Fig.6c indicates the area where the rod-like γ′ phase is distributed) (a) base metal (b) dendrite in weld metal (c) grain boundaries in weld metal |
|