Inconel 740H焊接接头不同温度蠕变后 γ′贫化区的形成及其对力学性能的影响 |
| 周任远, 朱丽慧 |
|
Formation of γ′-Denuded Zone and Its Effect on the Mechanical Properties of Inconel 740H Welded Joint After Creep at Different Temperatures |
| ZHOU Renyuan, ZHU Lihui |
| 图4 蠕变前和不同温度蠕变后IN 740H焊接接头的OM像 |
| Fig.4 OM images of IN 740H welded joints before (a) and after creep (b-g) at different temperatures (a) before creep (b) specimen 700-1 (c) specimen 700-2 (d) specimen 750-1(e) specimen 750-2 (f) specimen 800-1 (g) specimen 800-2 |
|