机械合金化AlCrCu0.5Mo0.5Ni高熵合金及其后续退火态的结构演化 |
| 雷云龙, 杨康, 辛越, 姜自滔, 童宝宏, 张世宏 |
|
Microstructure Evolution of Mechanically-Alloying and Its Subsequently-Annealed AlCrCu0.5Mo0.5Ni High-Entropy Alloy |
| LEI Yunlong, YANG Kang, XIN Yue, JIANG Zitao, TONG Baohong, ZHANG Shihong |
| 图13 球磨态和退火态MA粉末的力学性能 |
| Fig.13 Mechanical properties of MA powders in ball-milled and annealing states (H i represent MA powders annealed at i temperature) (a) load-depth curves (b) hardness and elasticity modulus |
|