机械合金化AlCrCu0.5Mo0.5Ni高熵合金及其后续退火态的结构演化 |
| 雷云龙, 杨康, 辛越, 姜自滔, 童宝宏, 张世宏 |
|
Microstructure Evolution of Mechanically-Alloying and Its Subsequently-Annealed AlCrCu0.5Mo0.5Ni High-Entropy Alloy |
| LEI Yunlong, YANG Kang, XIN Yue, JIANG Zitao, TONG Baohong, ZHANG Shihong |
| 图2 组成元素之间的混合焓 |
| Fig.2 Mixing enthalpies between component elements (unit: kJ/mol) |
|