TC4钛合金跨相区连续热压缩 α 相组织演变规律及织构形成机理 |
||||||||||||
| 赵焯雅, 孟令健, 林鹏, 曹晓卿 | ||||||||||||
|
Microstructure Evolution and Texture Formation Mechanism of α Phase During Continuous Through-Transus Thermal Compression of TC4 Titanium Alloy |
||||||||||||
| ZHAO Zhuoya, MENG Lingjian, LIN Peng, CAO Xiaoqing | ||||||||||||
| 表2 TC4钛合金在不同热压缩工艺下以0.01 s-1形变速率总压缩60%后的室温拉伸性能 |
||||||||||||
| Table 2 Tension properties of TC4 titanium alloy at room temperature after compression under different processing methods with a total compression of 60% at 0.01 s-1 |
||||||||||||
|
||||||||||||