B对Fe-Cr-B-C合金凝固行为、强韧性及耐磨性的影响 |
| 赵广迪, 李阳, 姚晓雨, 王亮, 李渭滨, 潘玉华, 李维娟, 王兆宇 |
|
Effect of Boron on Solidification Behavior, Strength-Toughness, and Wear Resistance of Fe-Cr-B-C Alloy |
| ZHAO Guangdi, LI Yang, YAO Xiaoyu, WANG Liang, LI Weibin, PAN Yuhua, LI Weijuan, WANG Zhaoyu |
| 图7 3种B含量Fe-Cr-B-C合金的差热分析(DTA)冷却曲线 |
| Fig.7 Differential thermal analysis (DTA) cooling curves of the Fe-Cr-B-C alloys with B contents of 0.0006% (a), 0.51% (b), and 2.89% (c) (Cooled from super-solidus temperature with cooling rate of 10 oC/min; P-C1, P-C2, and P-C3 represent the exothermic peaks) |
|