中碳Nb合金化钢液析碳化物的析出行为 |
| 梁炫, 侯廷平, 张东, 谭昕暘, 吴开明 |
|
Precipitation Behavior of Primary Carbides in Medium Carbon Nb-Alloyed Steel |
| LIANG Xuan, HOU Tingping, ZHANG Dong, TAN Xinyang, WU Kaiming |
| 图9 1.6Nb钢的溶质平衡分配系数随温度的变化 |
| Fig.9 Variation of solute equilibrium partition coeffici-ents kC (a) and kNb (b) with temperature for 1.6Nb steel |
|