中碳Nb合金化钢液析碳化物的析出行为 |
| 梁炫, 侯廷平, 张东, 谭昕暘, 吴开明 |
|
Precipitation Behavior of Primary Carbides in Medium Carbon Nb-Alloyed Steel |
| LIANG Xuan, HOU Tingping, ZHANG Dong, TAN Xinyang, WU Kaiming |
| 图8 凝固过程Thermo-Calc热力学计算Nb含量对相变的影响 |
| Fig.8 Effect of Nb content on phase transformation during solidification process by Thermo-Calc calculation (a) 0.1Nb (b) 0.6Nb (c) 1.1Nb (d) 1.6Nb |
|