中碳Nb合金化钢液析碳化物的析出行为 |
| 梁炫, 侯廷平, 张东, 谭昕暘, 吴开明 |
|
Precipitation Behavior of Primary Carbides in Medium Carbon Nb-Alloyed Steel |
| LIANG Xuan, HOU Tingping, ZHANG Dong, TAN Xinyang, WU Kaiming |
| 图5 NbC的电子总态密度和分态密度,及Nb、C的总态密度 |
| Fig.5 TDOS and PDOS for NbC (a), and TDOS for Nb (b) and C (c) |
|