中碳Nb合金化钢液析碳化物的析出行为 |
| 梁炫, 侯廷平, 张东, 谭昕暘, 吴开明 |
|
Precipitation Behavior of Primary Carbides in Medium Carbon Nb-Alloyed Steel |
| LIANG Xuan, HOU Tingping, ZHANG Dong, TAN Xinyang, WU Kaiming |
| 图4 NbC的声子谱及声子态密度 |
| Fig.4 Calculated phonon dispersion spectra (a) and total or partial density of states (TDOS, PDOS) (b) for NbC |
|