He泡液态金属铝的动态拉伸断裂机制与损伤模型
周婷婷, 赵福祺, 周洪强, 张凤国, 殷建伟

Mechanism and Damage Model for the Dynamic Tensile Fracture of Liquid Aluminum Containing He Bubbles
ZHOU Tingting, ZHAO Fuqi, ZHOU Hongqiang, ZHANG Fengguo, YIN Jianwei
图2 应变率为3.0 × 108 s-1时纯Al和含He泡铝样品在拉伸过程中的He泡与孔洞演化
Fig.2 Evolutions of He bubble/voids during the dynamic tension process at the strain rate (ε˙) of 3.0 × 108 s-1
(a) Al-He sample (b) pure Al