固溶态Mg-10Gd-6Y-1.5Zn-0.5Zr合金热加工图构建及微观组织演变 |
| 包成利, 李豪, 胡励, 周涛, 唐明, 何曲波, 刘相果 |
|
Construction of Hot Processing Map of Solutionized Mg-10Gd-6Y-1.5Zn-0.5Zr Alloy and Microstructure Evolution |
| BAO Chengli, LI Hao, HU Li, ZHOU Tao, TANG Ming, HE Qubo, LIU Xiangguo |
| 图10 图9变形样品中层状LPSO相扭折角度和再结晶晶粒分数统计 |
| Fig.10 Statistical analysis of kink angles (180°-θ) of lamellar LPSO phases and DRX grain fractions of deformed samples in Fig.9 (θ—kink band angle) |
|