固溶态Mg-10Gd-6Y-1.5Zn-0.5Zr合金热加工图构建及微观组织演变 |
| 包成利, 李豪, 胡励, 周涛, 唐明, 何曲波, 刘相果 |
|
Construction of Hot Processing Map of Solutionized Mg-10Gd-6Y-1.5Zn-0.5Zr Alloy and Microstructure Evolution |
| BAO Chengli, LI Hao, HU Li, ZHOU Tao, TANG Ming, HE Qubo, LIU Xiangguo |
| 图6 固溶态Mg-10Gd-6Y-1.5Zn-0.5Zr合金不同应变下的三维功率耗散系数图 |
| Fig.6 3D power dissipation coefficient (η) maps of solid-solution Mg-10Gd-6Y-1.5Zn-0.5Zr alloys under 0.1 (a), 0.3 (b), 0.5 (c), and 0.7 (d) strains |
|