纳米ZrB2 增强CoNiCrAlY复合粉末的机械合金化制备及其涂层的组织与性能 |
| 杨康, 辛越, 姜自滔, 刘侠, 薛召露, 张世宏 |
|
Mechanical Alloying Fabrication of Nano-ZrB2-Reinforced CoNiCrAlY Composite Powders and Microstructure-Property Characterization of the Resultant Coatings |
| YANG Kang, XIN Yue, JIANG Zitao, LIU Xia, XUE Zhaolu, ZHANG Shihong |
| 图11 不同温度下MA-1涂层的磨损表面形貌SEM像 |
| Fig.11 Low (a, c, e) and high (b, d, f) magnified SEM images of worn surface morphologies of the MA-1 coatings at different temperatures (a, b) 550 oC (c, d) 750 oC (e, f) 950 oC |
|