纳米ZrB2 增强CoNiCrAlY复合粉末的机械合金化制备及其涂层的组织与性能 |
| 杨康, 辛越, 姜自滔, 刘侠, 薛召露, 张世宏 |
|
Mechanical Alloying Fabrication of Nano-ZrB2-Reinforced CoNiCrAlY Composite Powders and Microstructure-Property Characterization of the Resultant Coatings |
| YANG Kang, XIN Yue, JIANG Zitao, LIU Xia, XUE Zhaolu, ZHANG Shihong |
| 图10 不同温度下CoNiCrA1Y涂层的磨损表面形貌SEM像 |
| Fig.10 Low (a, c, e) and high (b, d, f) magnified SEM images of worn surface morphologies of the CoNiCrA1Y coatings at different temperatures (a, b) 550 oC (c, d) 750 oC (e, f) 950 oC |
|