纳米ZrB2 增强CoNiCrAlY复合粉末的机械合金化制备及其涂层的组织与性能 |
| 杨康, 辛越, 姜自滔, 刘侠, 薛召露, 张世宏 |
|
Mechanical Alloying Fabrication of Nano-ZrB2-Reinforced CoNiCrAlY Composite Powders and Microstructure-Property Characterization of the Resultant Coatings |
| YANG Kang, XIN Yue, JIANG Zitao, LIU Xia, XUE Zhaolu, ZHANG Shihong |
| 图7 3种涂层在不同温度下的摩擦系数(COF)曲线 |
| Fig.7 Coefficient of friction (COF) curves at different temperatures of CoNiCrAlY (a), MA-1 (b), and MA-2 (c) coatings (t—time) |
|