纳米ZrB2 增强CoNiCrAlY复合粉末的机械合金化制备及其涂层的组织与性能 |
| 杨康, 辛越, 姜自滔, 刘侠, 薛召露, 张世宏 |
|
Mechanical Alloying Fabrication of Nano-ZrB2-Reinforced CoNiCrAlY Composite Powders and Microstructure-Property Characterization of the Resultant Coatings |
| YANG Kang, XIN Yue, JIANG Zitao, LIU Xia, XUE Zhaolu, ZHANG Shihong |
| 图2 球磨不同时间后MA-1、MA-2复合粉末的平均粒径(D50)及筛分后质量占比 |
| Fig.2 Average diameters (D50) (a) and percentages after sieving (b) of MA-1 and MA-2 composite powders after different ball milling time |
|