TRIP型双相不锈钢Fe-19.6Cr-2Ni-2.9Mn-1.6Si的微裂纹形核及扩展 |
| 张文彬, 李小龙, 郝硕, 刘胜杰, 蔡星周, 陈雷, 金淼 |
|
Microcrack Nucleation and Propagation of TRIP-Assisted Duplex Stainless Steel Fe-19.6Cr-2Ni-2.9Mn-1.6Si |
| ZHANG Wenbin, LI Xiaolong, HAO Shuo, LIU Shengjie, CAI Xingzhou, CHEN Lei, JIN Miao |
| 图10 微裂纹形核特征示意图 |
| Fig.10 Schematics of microcrack nucleation characteristics (a) nucleation at the intersection position of transformed martensite/ferrite/residual austenite (b) nucleation at the intersection position of the ferrite/martensite phase boundary and ferrite grain boundary (c) nucleation at the intersection of ferrite/martensite phase boundary and original austenite grain boundary |
|