TRIP型双相不锈钢Fe-19.6Cr-2Ni-2.9Mn-1.6Si的微裂纹形核及扩展 |
| 张文彬, 李小龙, 郝硕, 刘胜杰, 蔡星周, 陈雷, 金淼 |
|
Microcrack Nucleation and Propagation of TRIP-Assisted Duplex Stainless Steel Fe-19.6Cr-2Ni-2.9Mn-1.6Si |
| ZHANG Wenbin, LI Xiaolong, HAO Shuo, LIU Shengjie, CAI Xingzhou, CHEN Lei, JIN Miao |
| 图2 Fe-19.6Cr-2Ni-2.9Mn-1.6Si钢初始组织特征 |
| Fig.2 Initial microstructure of the as-received Fe-19.6Cr-2Ni-2.9Mn-1.6Si steel (a) SEM image (b) phase distribution (c) inverse pole figure (IPF) |
|