汽车用齿轮钢16MnCrS5热处理变形机理 |
| 屈小波, 安金敏, 王林, 李喜 |
|
Quenching Deformation of the 16MnCrS5 Gear Steel for Automobile |
| QU Xiaobo, AN Jinmin, WANG Lin, LI Xi |
| 图14 淬火变形后16MnCrS5齿轮钢微观组织表征 |
| Fig.14 Microstructure characterizations of the quench-ing deformed 16MnCrS5 gear steel (a) SEM image (b) EBSD inverse pole figure (IPF) grain orientation map (c) corresponding kernel average misorientation (KAM) map |
|