汽车用齿轮钢16MnCrS5热处理变形机理 |
| 屈小波, 安金敏, 王林, 李喜 |
|
Quenching Deformation of the 16MnCrS5 Gear Steel for Automobile |
| QU Xiaobo, AN Jinmin, WANG Lin, LI Xi |
| 图9 淬火变形实验和数值模拟获得的16MnCrS5齿轮钢C型缺口试样淬火变形量随带状组织等级变化 |
| Fig.9 Quenching deformations of the 16MnCrS5 C-notch samples obtained by experiment and simulation as function of band structure grade (TD—transverse direction, RD—rolling direction) |
|